{"id":3813,"date":"2026-11-20T01:10:34","date_gmt":"2026-11-19T17:10:34","guid":{"rendered":"http:\/\/www.ciel-j.com\/blog\/?p=3813"},"modified":"2026-11-20T01:10:34","modified_gmt":"2026-11-19T17:10:34","slug":"what-is-sink-mark-in-injection-molding-4524-ae63e9","status":"publish","type":"post","link":"http:\/\/www.ciel-j.com\/blog\/2026\/11\/20\/what-is-sink-mark-in-injection-molding-4524-ae63e9\/","title":{"rendered":"What is sink mark in injection molding?"},"content":{"rendered":"<p>Hey everyone, if you\u2019ve ever worked with injection molding parts, chances are you\u2019ve run into sink marks at some point \u2014 and let\u2019s be real, they\u2019re such a headache. As someone who\u2019s been running an injection molds supplier for over a decade, I\u2019ve seen clients pull their hair out over these tiny (or not-so-tiny) imperfections ruining parts that otherwise look great. Today, let\u2019s break down what sink marks actually are, why they happen, and what you can do about them \u2014 plus how partnering with the right mold shop can make all the difference. <a href=\"https:\/\/www.jiejinplastic.com\/injection-molding\/injection-molds\/\">Injection Molds<\/a><\/p>\n<p><img decoding=\"async\" src=\"https:\/\/www.jiejinplastic.com\/uploads\/49143\/small\/led-light-bottom-plastic-housing81a0d.jpg\"><\/p>\n<p>First, let\u2019s keep it simple: a sink mark is that shallow, dimpled indent you see on the surface of an injection molded part, usually right next to a thick section, rib, boss, or any other feature that\u2019s bulkier than the surrounding material. Think of it like a sunken patch on a car door panel, or a subtle dip on the back of a plastic enclosure for a gadget. It\u2019s not a scratch, it\u2019s not a bubble \u2014 it\u2019s totally tied to how the plastic cools and shrinks inside the mold.<\/p>\n<p>Here\u2019s the science part, no stuffy textbook jargon, I promise. When you inject molten plastic into a mold, the part starts cooling from the outside in. The thin outer layer touches the cold mold walls first, so it hardens quickly. The middle of the part \u2014 especially those extra-thick spots like ribs \u2014 stays molten longer. As the plastic cools, all plastics shrink, right? Like how a chocolate bar gets smaller when it goes from warm to cold. But the outer skin is already rigid, so when the thick inner core shrinks, it pulls the rigid outer layer inward. That\u2019s what creates the sink mark.<\/p>\n<p>Wait, why do some parts have zero sink marks and others have five? It all comes down to mold design, material choice, process settings, and even part geometry. Let\u2019s break down the most common causes I see day to day, since that\u2019s what clients usually come to me asking about.<\/p>\n<p>First up, part geometry mistakes. If you have a 2mm thick wall and a 6mm rib that\u2019s way thicker than the main part, that\u2019s a recipe for a sink mark. The rib is so bulky that it cools way slower than the main wall, so the shrinkage there pulls on the surface. I had a client last year who came to me with a batch of custom plastic housings for power tools \u2014 they\u2019d designed a 5mm rib to add strength, but it created such a big sink on the front of the housing that it couldn\u2019t pass their quality checks. We fixed it by adding a fillet to the base of the rib to spread the material out, and even reduced the rib thickness to 3mm (keeping the strength up) \u2014 no more sinks.<\/p>\n<p>Next, mold design issues. Sometimes the mold itself doesn\u2019t give the plastic enough room to pack. Packing is that step where you inject extra molten plastic into the mold right after the initial shot, to fill in gaps from shrinkage. If your mold has thin gates (the openings where plastic flows in) or the cooling lines aren\u2019t placed right, the plastic can\u2019t flow enough to pack the thick sections. I\u2019ve seen cheap, poorly made molds with cooling lines only around the outer edges \u2014 the thick ribs have no cooling at all, so they stay molten forever and shrink more, leading to worse sinks. A good mold shop will place cooling lines directly next to thick features like ribs and bosses to keep them at the same temperature as the rest of the part, so they cool evenly.<\/p>\n<p>Then there\u2019s process settings. Even a great mold can have sink marks if you\u2019re not tuning the injection molding machine right. Too low a melt temperature? The plastic might harden too fast, so you can\u2019t pack enough material into the thick spots. Too low a packing pressure? No extra plastic to fill in the shrinkage gaps. Too short a cooling time? The part gets ejected before it\u2019s fully solid, so it deforms as it cools in air. I once had a client who thought their mold was bad, but when we checked their machine settings, their packing pressure was set to half what it should be. Cranking that up just fixed the sink marks \u2014 they didn\u2019t even need a new mold.<\/p>\n<p>Material choice plays a role too. Some plastics shrink more than others. Polyethylene (PE) and polypropylene (PP) are common in packaging and household parts, and they shrink a lot compared to engineering plastics like ABS or nylon. If you\u2019re using a high-shrink material for a part with big thick ribs, you\u2019re way more likely to get sink marks. There are also modified materials \u2014 like filled plastics (with glass fibers or minerals) that shrink less, so they\u2019re better for parts where surface finish matters. I always tell clients to pick a material that matches their part\u2019s needs, not just the cheapest one, if surface quality is a priority.<\/p>\n<p>Now, the big question: how do you fix sink marks? It\u2019s not a one-size-fits-all solution, which is why working with a good injection molds supplier is key. Let\u2019s go over the fixes I recommend most often, based on what\u2019s causing the issue.<\/p>\n<p>If it\u2019s part geometry: modify thick features to be thinner, add fillets to their bases, or offset them so they don\u2019t line up with thin wall sections. For example, instead of a big rib running straight across a thin wall, split it into smaller, thinner ribs \u2014 that reduces the mass, so it cools more evenly. I did this for a client making electronic device covers; they had a single 4mm rib that caused a visible sink, so we split it into two 2mm ribs spaced apart, and the surface was smooth enough for their product.<\/p>\n<p>If it\u2019s mold design: adjust cooling lines to be closer to thick sections, use bigger gates to improve plastic flow into thick areas, or even add a \u201csink mark relief\u201d feature \u2014 a small indent on the opposite side of the part where the sink would be, so it doesn\u2019t show on the finished surface. Wait, that\u2019s a trick I use all the time. If the sink is going to be on the back of a part that no one sees, we just make the mold slightly recessed there, so when the plastic shrinks, it dips into that recess instead of the front. Saves a ton of time and cost vs. reworking the whole mold.<\/p>\n<p>If it\u2019s process: tweak packing pressure, hold time, cooling time, or melt temperature. Sometimes just extending the packing hold time by a few seconds lets more plastic flow in to fill the shrinkage gap. I\u2019ve seen that fix 90% of minor sink marks without touching the mold at all.<\/p>\n<p>But wait, there are some cases where sink marks are totally unavoidable, right? If you need a thick section for strength, and the surface has to be smooth, then you have to plan for it from the start. That\u2019s where a good mold shop comes in \u2014 we don\u2019t just build a mold and hope for the best; we design around your part\u2019s requirements. For example, if a medical device needs a smooth surface (no sinks allowed) and a thick boss to attach a component, we\u2019ll design the mold with extra cooling around that boss, use a larger gate, and pick a low-shrink material \u2014 all before we even cut steel.<\/p>\n<p>Now, let\u2019s talk about why sink marks matter more than just \u201cthey look bad.\u201d If you\u2019re making a structural part, a sink mark can be a sign of uneven cooling that makes the part weaker. Or if it\u2019s a sealed part, a sink might create a gap where liquid or dust can get in. For consumer products, even a tiny sink can make your product look cheap, which kills sales. I had a startup client a few years back \u2014 they were making a smart water bottle, and their first batch had subtle sinks on the main body. Retailers rejected them because the parts looked \u201cflawed,\u201d so they came to us to rework the mold. We fixed the geometry and mold design, and they ended up landing a big retail deal because the surface finish was perfect. That\u2019s why sink marks aren\u2019t just a cosmetic issue \u2014 they can impact your product\u2019s success.<\/p>\n<p>I\u2019ve seen so many clients go for the cheapest mold shop, only to end up with parts full of sink marks that cost way more to fix later. A good injection molds supplier will walk you through part design, material selection, mold design, and process optimization to minimize or eliminate sink marks. We test the mold before shipping it, run trial shots, and adjust settings so you don\u2019t have to do all that guesswork. That\u2019s the value we bring \u2014 not just building a mold, but making sure it works for your specific parts.<\/p>\n<p><img decoding=\"async\" src=\"https:\/\/www.jiejinplastic.com\/uploads\/49143\/small\/plastic-battery-housing7d13f.jpg\"><\/p>\n<p>If you\u2019re dealing with sink marks on your injection molded parts, or you\u2019re planning a new project and want to avoid them in the first place, don\u2019t hesitate to reach out. We\u2019ve worked with everything from small startups to big manufacturers, and we can help you figure out the root cause, fix it, and make sure your parts meet your quality standards. Whether you need to rework an existing mold, design a new one, or just get advice on material choices, we\u2019re here to make the process smoother.<\/p>\n<p><a href=\"https:\/\/www.jiejinplastic.com\/plastic-tableware\/plastic-tableware-set\/\">Plastic Tableware Set<\/a> References:<\/p>\n<ol>\n<li>Rosato, D. V., &amp; Rosato, M. G. (2000). Injection Molding Handbook. Kluwer Academic Publishers.<\/li>\n<li>Crawford, R. J. (1998). Plastics Engineering. Butterworth-Heinemann.<\/li>\n<li>Groover, M. P. (2020). Fundamentals of Modern Manufacturing: Materials, Processes, and Systems. John Wiley &amp; Sons.<\/li>\n<\/ol>\n<hr>\n<p><a href=\"https:\/\/www.jiejinplastic.com\/\">Huizhou Jiejin Plastic Technology Co., Ltd.<\/a><br \/>Huizhou Jiejin Plastic Technology Co., Ltd. is one of the most professional injection molds manufacturers and suppliers in China, featured by quality products and low price. We warmly welcome you to wholesale advanced injection molds made in China here from our factory. If you have any enquiry about customized service and OEM service, please feel free to email us.<br \/>Address: Guangming Village, Tongqiao Town, Huizhou City, Guangdong Province, China<br \/>E-mail: info@jiejinplastic.com<br \/>WebSite: <a href=\"https:\/\/www.jiejinplastic.com\/\">https:\/\/www.jiejinplastic.com\/<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Hey everyone, if you\u2019ve ever worked with injection molding parts, chances are you\u2019ve run into sink &hellip; <a title=\"What is sink mark in injection molding?\" class=\"hm-read-more\" href=\"http:\/\/www.ciel-j.com\/blog\/2026\/11\/20\/what-is-sink-mark-in-injection-molding-4524-ae63e9\/\"><span class=\"screen-reader-text\">What is sink mark in injection molding?<\/span>Read more<\/a><\/p>\n","protected":false},"author":973,"featured_media":3813,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[3776],"class_list":["post-3813","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-industry","tag-injection-molds-498c-af14a7"],"_links":{"self":[{"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/posts\/3813","targetHints":{"allow":["GET"]}}],"collection":[{"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/users\/973"}],"replies":[{"embeddable":true,"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/comments?post=3813"}],"version-history":[{"count":0,"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/posts\/3813\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/posts\/3813"}],"wp:attachment":[{"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/media?parent=3813"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/categories?post=3813"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.ciel-j.com\/blog\/wp-json\/wp\/v2\/tags?post=3813"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}